Quick answer
My coals show a fault: what could cause it, and what do I send so it can be checked?
A fault in hookah coals has several possible causes, in production, in transport or in use; the triage table lists them by symptom. Each row ends with what the quality control desk needs to see, and a cause is confirmed only against the batch. Find your symptom, gather what its row asks for, and send it with the carton marks, so that the report can be tied to one batch.
1. Triage table: symptom, possible causes, what to send
Find the symptom in the first column. The two middle columns list what could cause it, on the factory's side and after the container left; the last column is what to send.
Definition
coal fault
A coal fault is a defect that can be observed in a hookah coal, such as a crack, breakage, a smell on warming up, heavy ash, a short burn or uneven size.
| Symptom | Possible causes in production | Possible causes in transport or use | What to send |
|---|---|---|---|
| Cracks or broken pieces | Pressing or drying of the batch | Drops, crushed cartons or damp on the way; how the coals were heated | Photos of the pieces and of the carton they came from; the number of cartons affected |
| Smell or smoke on warming up | The raw material or the drying of the batch | Damp taken up in storage; residue on the heater | A short video of pieces warming up on a clean electric coil; how the cartons were stored |
| More ash than expected | The ash of the batch against the grade ordered | A comparison by eye with another product or another setup | A photo of the ash from a counted number of pieces; the grade on your order |
| Short burn | The density or the size of the pieces | A heat source or setup that differs from the one the sample was tested on | The burn time of three pieces on one heat source; the measured size of the pieces |
| Slow to light | The density or the moisture of the batch | Damp taken up in storage; a weaker heat source | The time to light on one heat source; how the cartons were stored |
| Uneven size or weight | The mold or the cutting of the batch | — | Caliper readings of ten pieces from three cartons; the count of pieces in one kilogram |
| Damp or soft cartons | — | Condensation or water in the container | Photos at the open doors before unloading; the seal number; where the cartons stood |
Caution
Every cause in the table is a possibility. Which one applies to your coals is known only after the report has been checked against the batch.
2. Before you report a fault
A report that can be checked needs no second round of questions. Four steps make it checkable.
-
Test on one heat source
Use the same heat source for every piece you test, and say which one it was. The factory's own burn test is run like this: three pieces are lit on an electric coil, and the time to light and the burn time are recorded.
-
Compare with your reference sample
Test pieces from the sealed sample of the run you approved beside pieces from the container, on the same day and in the same way.
-
Note the carton marks
Write down the marks and the production date on every carton the pieces came from. They tie your report to one batch.
-
Count what is affected
Open cartons from the front, the middle and the back of the load, and give the number of cartons checked and the number with the fault.
The same tests, with the same record, are on the sample test sheet. The figures to measure against are the ones you wrote on the specification sheet before the order.
3. What the factory checks on its side
The factory checks a report against its own record of the batch and against the sample it kept.
- The factory fails a batch on smell or smoke on warming up.
- The factory fails a batch on high ash.
- The factory fails a batch on cracks or breakage.
- The factory fails a batch on uneven size or density.
The factory keeps a sample of about 25 kg from every batch for 5 years. Pieces from that sample can be tested beside the ones you report. Its drop test is run like this: lit pieces are dropped onto a hard tiled floor, from 100 cm for cubes and from 30 cm for hexagonal, dome and finger shapes.
The desk is run by Sri Wahyuni, Quality Control Supervisor. A fault that shows in the retained sample points to the batch. A fault that does not show there points to what happened after loading, and the report is read again with that in mind. How two runs are kept alike is on the page about consistency between orders.
Note
The table and the checks say where to look. They do not say in advance whose fault a problem is.
4. Report it: arrival sheet or claim form
Two sheets carry a report, and which one to use depends on when the fault shows.
- A container that has just arrived: fill in the arrival sheet while it is unloaded. It records the seal, the carton count and a measured sample of cartons.
- A fault you want the factory to answer for: send the claim form on the page about complaints and claims, with the evidence the table asks for.
A claim has a time limit. The factory accepts a claim on quantity within one week and on quality within two weeks of the container's arrival at the buyer's warehouse. Report a fault as soon as it shows, even if you have not finished the tests.
Tip
Keep the cartons the faulty pieces came from, closed and dry, until the report has been answered.